Galvanizing Vent & Drain Hole Finder
Drop in a STEP file of your weldment. The tool finds every closed tube and pipe, works out where the vent and drain holes go for the way the part hangs in the kettle, and sizes them from the American Galvanizers Association rules.
Find the closed sections before the kettle does.
Your file is read right here in your browser. It is not uploaded anywhere.
No file loaded yet.
- Closed member: needs holes
- Has an open end
- Vent (high)
- Drain (low)
- Opening already in the model
Trapped liquid turns to steam.
It can blow apart
Cleaning solution or rinse water trapped in a closed section flashes to steam in the zinc bath. AGA puts the pressure at up to 3,600 psi, enough to rupture the part and put the galvanizer’s crew at risk.
Air has to get out
A closed part floats and traps air, so zinc cannot reach the inside. Vents at the high point let the air out; drains at the low point let the zinc run back out.
Holes go high and low
Parts go into the kettle at an angle. Vents go at the highest point and drains at the lowest, at both ends of every closed section, and should be visible from the outside.
What it finds, and the rules it uses.
Finding the hollow members. Every solid in the file is checked for an outer and inner wall around one axis: round tube and pipe, and square and rectangular tube. Then the tool looks down the inside of each one from the middle to both ends. If the end is open, it vents itself. If another part closes it, that end is sealed. If it runs into the hollow of another tube, as at an open miter or tee, the two are one enclosed section.
Placing the holes. Each sealed member end gets two holes 180° apart, one on the high side and one on the low side as the part hangs, 1/2 inch from the end of the wall so they sit close to the weld. Every enclosed section also needs an opening at its highest point and at its lowest point. An open end or a hole already in the model counts; where there is none, the tool adds a vent or a drain.
| Member | Hole size | Source |
|---|---|---|
| Round tube and pipe under 3 in OD | 25% of the inside diameter, at least 3/8 in | AGA design guide, pipe-work Fig. 21 |
| Round tube and pipe 3 in OD and up | The two holes at an end give 30% of the inside area | AGA design guide p.14 |
| Square and rectangular tube | The two holes at an end give 30% of the inside area | AGA design guide p.13, tube truss members |
Sources: American Galvanizers Association, The Design of Products to be Hot-Dip Galvanized After Fabrication (2023), which draws on ASTM A385. We read “30% of the cross-sectional area” as the inside (open) area of the tube. Holes are rounded up to the next 1/16 inch.
What it can read. STEP files (AP203, AP214, AP242) with each member as its own solid, the way a weldment or multibody part exports. A frame saved as one fused solid shows up as plain steel. It does not check lapped plates, tanks, or holes drilled through into the next member, and it does not know how your galvanizer will hang the part.
Check with your galvanizer. This marks the published minimums at the obvious places. Long members, internal stiffeners and the galvanizer’s own rigging can call for bigger or extra holes. Send them the drawing before you drill. Need parts built ready to galvanize? Ask us for a quote.